2024知到答案 Weldability of Metals and Alloys金属焊接性 最新智慧树满分章节测试答案
第一章 单元测试
1、单选题:
With carbon equivalent ( ), the steel has a low tendency to harden and cold cracking?
选项:
A:less than 0.40%
B:less than 0.60%
C:less than 0.50%
D:less than 0.80%
答案: 【less than 0.40%】
2、单选题:
( ) is not a factor that affects weldability.
选项:
A:Welding process
B:joint type
C:chemical composition
D:operation skill
答案: 【operation skill】
3、多选题:
The calculation formula of carbon equivalent of the IWS considers the influence of () on weldability.
选项:
A:welding structure 
B:diffusion hydrogen
C:welding process
D:chemical composition
答案: 【welding structure
diffusion hydrogen;
welding process】
4、单选题:
Maximum crack distance has been used to allow more accurate determination of the cracking ( ) range.
选项:
A:size
B:temperature
C:toughness
D:strength
答案: 【temperature】
5、多选题:
Weldability is not easily quantified, and can depend on a variety of factors, including ( ).
选项:
A:welding method
B:operator and welder
C:physical specifics of the joint
D:welded structure
答案: 【welding method;
physical specifics of the joint;
welded structure】
第二章 单元测试
1、单选题:
The weldability of high-carbon steel is worse than that of low-carbon steel because high-carbon steel is with ( ).
选项:
A:higher toughness
B:lower melting point
C:higher carbon content
D:higher sulphur content
答案: 【higher carbon content】
2、单选题:
Normally, because of auto-tempering, the postweld microstructure of QTLA steel is ( ).
选项:
A:high carbon martensite
B:upper bainite
C:tempered martensite
D:ledeburite
答案: 【tempered martensite】
3、多选题:
QTLA steel is not susceptible to solidification cracking because it is with ( ).
选项:
A:low impurity content
B:low nickel content
C:low carbon content
D:low manganese content
答案: 【low impurity content;
low carbon content】
4、多选题:
For HTLA steels, chromium is able to ( ).
选项:
A:decrease toughness of HTLA steels
B:increase toughness of HTLA steels
C:increase hardeness of HTLA steels
D:decrease hardeness of HTLA steels
答案: 【decrease toughness of HTLA steels;
increase hardeness of HTLA steels】
5、判断题:
When you weld HTLA steels, you'd better to take advantage of auto-tempering.
选项:
A:错
B:对
答案: 【错】
6、多选题:
Auto-tempering occurs after welding when ( ).
选项:
A:peak temperature is high
B:cooling rate is slow
C:Ms is high
D:carbon content of weld is low
答案: 【cooling rate is slow;
carbon content of weld is low】
7、判断题:
Before designing welding procedure, we'd better to analyze the weldability of the workpiece.
选项:
A:错
B:对
答案: 【对】
8、判断题:
To remedy the underbead cracking, we need to reduce cooling rate when we weld oil engine connecting rod.
选项:
A:对
B:错
答案: 【对】
9、单选题:
If the carbon content of a type of steel is 0.1%, this steel is a kind of ( ).
选项:
A:medium-carbon steel
B:HTLA steel
C:low-carbon steel
D:high-carbon steel
答案: 【low-carbon steel】